I'm logging on and asking this question for a co-worker. She wants help fixing her deck. Here's what she says:
"Last year, I had a new deck built at my townhouse. About two months after construction I coated the wood with a BEHR waterproofer. I thought followed the instructions on the can. A little over a year later, and the wood is buckling on the deck surface and handrails. I asked the deck-builder to take a look at it, and he told me I must have put the stain on wrong. I'm not sure what to think.
Any idea on what the problem is, how to fix it, and how to prevent it from happening again?"
"Last year, I had a new deck built at my townhouse. About two months after construction I coated the wood with a BEHR waterproofer. I thought followed the instructions on the can. A little over a year later, and the wood is buckling on the deck surface and handrails. I asked the deck-builder to take a look at it, and he told me I must have put the stain on wrong. I'm not sure what to think.
Any idea on what the problem is, how to fix it, and how to prevent it from happening again?"




) but because I have had very good success with their products over a long time span. Most of the upper end sealers are pretty good.
Little about a lot and a lot about a little.
Comment